A. Improve bonding
B. Decrease porosity
C. They react with the porcelain opaque layer, which masks the metal
D. Improves the thermal expansion between the metal and porcelain
Advertisement
Related Mcqs:
- Indium in metal alloys_______________?
- A. Improve bonding B. Harden the metal ceramic Ag-Pd alloy C. Both A and B D. None of the above...
- Ideal requirement of metal ceramic casting____________?
- A. Low fusing ceramic and high fusing alloys B. Matching of coefficients of thermal expansion of ceramics and alloy C. Bonding between ceramic and alloy D. All of the above...
- Gallium and indium added to Amalgam replace______________?
- A. Silver B. Tin C. Mercury D. Zinc...
- Coefficient of thermal expansion of metal-ceramic alloys is________________?
- A. Same as porcelain B. More than porcelain C. Less than porcelain D. More than or equal to porcelain but not less...
- The anatomic crown is shorter than the clinical crown of a tooth in which of the following instances___________________?
- A. Impaction B. Gingivitis C. Occlusal wear D. Gingival recession...
- Porcelain binds to metal in PFM crown by_________________?
- A. Metallic bind B. Transparency C. Chemical bond D. B and C...
- For porcelain fused to metal crown, the porcelain should have ______________?
- A. High fusion expansion B. High fusion temperature C. Linear coefficient of thermal expansion less than that of metal D. Linear coefficient of thermal expansion more than that of metal...
- The castability of chromium-cobait base metal alloys when compared to gold based noble metal alloys is_______________?
- A. More B. Less C. Equal D. Depends on the alloy type...
- Linear coefficient of thermal expansion of metal used for metal caramic restoration range from________________?
- A. 11.5-12.5×10-6/°C B. 10.5-11.5×10-6/°C C. 13.5-14.5×10-6/°C D. 16.5-17.5×10-6/°C...
- By product of condensation reaction between silicone base and alkyl silicate in presence of tin octate_______________?
- A. Ethyl alcohol B. Glycol C. Acetate D. Propanolol...