A. 8
B. 24
C. 44
D. 58
Advertisement
Related Mcqs:
- 10 to 30% magnesite is added to Chromite to produce chrome-magnesite refractories. Magnesite addition is mainly done to improve the _____________ of Chromite?
- A. Spalling resistance B. Refractoriness C. Crushing strength D. Resistance to slag...
- Porosity of silica bricks varies from ______________ percent?
- A. 5 to 10 B. 20 to 30 C. 45 to 60 D. 60 to 75...
- Firing temperature of magnesite bricks is about _____________ °C?
- A. 800-1000 B. 1000-1200 C. 1600-1800 D. 2400-2600...
- Magnesite bricks have poor resistance to attack by _____________ slag?
- A. Lime B. Basic C. Acid D. None of these...
- Chrome magnesite bricks are_________________?
- A. Acidic in nature B. Neutral in nature C. Having higher RUL than silica bricks D. Made by mixing 30% Chromite and 70% Periclase...
- Chrome magnesite bricks are used in the_________________?
- A. Side walls of soaking pits and arc furnaces B. Copper melting furnaces & converters C. Burner block of glass tanks D. All A., B. and C....
- Magnesite chrome bricks are used in the___________________?
- A. Roof lining of basic open hearth & other basic furnaces B. Reheating furnaces C. Soaking pits D. All A., B. and C....
- Which of the following impurities reduces the refractoriness of magnesite bricks ?
- A. Al2O3 B. CaO C. SiO2 D. All A., B. & C....
- Magnesite bricks are used in those parts of furnaces, which are __________________?
- A. Subjected to temperature fluctuation B. Required to resist corrosive basic slag C. Subjected to high load D. None of these...
- High porosity refractory bricks have _______________?
- A. Poor resistance to the penetration of molten slag, metal & flue gases B. Poor heat conductivity & low strength C. Better thermal spalling resistance D. All A., B. and C....