A. 0.3
B. 0.5
C. 0.8
D. 2.5
Related Mcqs:
- Straight silicon steel (containing Si from 0.5 to 5%) because of their low hysteresis loss and high magnetic permeability are used for electrical appliances. Which of the following electrical appliances made of silicon steel contains maximum percentage of silicon (about 4%) ?
A. Armature of small motors/generators
B. Generators and small motors
C. Induction motors
D. High frequency transformers - Chilled iron castings are__________________?
A. Easily machinable
B. Soft on surface
C. Highly wear resistant
D. None of these - Silicon percentage in acid resistant cast iron is about________________?
A. 4
B. 8
C. 14
D. 20 - A hardness depth of about 3 mm can be achieved by induction hardness in ______________ seconds?
A. 5
B. 100
C. 250
D. 500 - The heat treatment process to which castings and the steel balls produced by cold heading are subjected is____________________?
A. Tempering
B. Normalising
C. Annealing
D. None of these - Containers made of high silicon cast iron (14% Si) are not suitable for the storage of ____________________?
A. Acetic acid
B. Benzoic & boric acids
C. Phosphoric acid (95%) & sulphuric acid (95%)
D. Hydrochloric acid (concentrated) - ______________ iron is produced, when molten pig iron is allowed to cool gradually?
A. White cast
B. Grey cast
C. Wrought
D. None of these - White cast iron as compared to grey cast iron is ________________?
A. More durable
B. Very brittle
C. Very hard
D. All A., B. & C. - _____________ iron is produced, when molten pig iron is chilled suddenly?
A. White cast
B. Grey cast
C. Wrought
D. None of these - The impure iron (pig iron) that is tapped out from blast furnace contains about _____________ percent carbon?
A. 0.2
B. 2
C. 4
D. 8