A. 800-1000
B. 1000-1200
C. 1600-1800
D. 2400-2600
Related Mcqs:
- 10 to 30% magnesite is added to Chromite to produce chrome-magnesite refractories. Magnesite addition is mainly done to improve the _____________ of Chromite?
A. Spalling resistance
B. Refractoriness
C. Crushing strength
D. Resistance to slag - Maximum apparent porosity of magnesite bricks is about _____________ percent?
A. 8
B. 24
C. 44
D. 58 - Magnesite bricks have poor resistance to attack by _____________ slag?
A. Lime
B. Basic
C. Acid
D. None of these - Firing temperature is minimum (1250-1400 °C) for _______________ bricks?
A. Fireclay
B. Direct bonded basic
C. Silica
D. Magnesite - Chrome magnesite bricks are_________________?
A. Acidic in nature
B. Neutral in nature
C. Having higher RUL than silica bricks
D. Made by mixing 30% Chromite and 70% Periclase - Chrome magnesite bricks are used in the_________________?
A. Side walls of soaking pits and arc furnaces
B. Copper melting furnaces & converters
C. Burner block of glass tanks
D. All A., B. and C. - Magnesite chrome bricks are used in the___________________?
A. Roof lining of basic open hearth & other basic furnaces
B. Reheating furnaces
C. Soaking pits
D. All A., B. and C. - Which of the following impurities reduces the refractoriness of magnesite bricks ?
A. Al2O3
B. CaO
C. SiO2
D. All A., B. & C. - Magnesite bricks are used in those parts of furnaces, which are __________________?
A. Subjected to temperature fluctuation
B. Required to resist corrosive basic slag
C. Subjected to high load
D. None of these - The maximum linear expansion of silica bricks during firing is about ______________ percent?
A. 0.5
B. 1
C. 2
D. 3.5